Magnetic Shielding Alloy - Rod Last updated
September 17 2021
Ni77/Fe14/Cu 5/Mo 4 NI037910

1 of 1

If the item shown is not exactly what you require please let us know by sending us a message
Diameter : 6.35mm
Harmful - Click here for further details    Irritant - Click here for further details   
To obtain optimum magnetic properties, this material should be magnetically annealed. This service is available on request.
 
Click on a price to add to shopping cart ( Prices are in USD)
Size
Order Code Length 1 pc 2 pcs 5 pcs 10 pcs
415-196-28 100 mm USD 302.00 USD 373.00 USD 530.00 USD 783.00 ?
572-291-28 200 mm USD 360.00 USD 456.00 USD 758.00   ?
632-978-94 500 mm USD 476.00 USD 717.00     ?
401-482-65 1000 mm USD 704.00       ?
 
 
Click on a price to add to shopping cart ( Prices are in USD)

Packing Packing costs are included in the price.
Terms of shipment Prices include delivery but not local taxes
Technical Data for     Magnetic Shielding Alloy       Rod
Typical Analysis : (ppm) Cu 5%, Fe 14%, Mo 4%, Ni + Co balance.
Intracom 7505 12 00 ( 2.9%)
US tariff code 7505 12 1000 ( 3%)
Tolerances
  Diameter:   =<10mm   ±10%
    Polymer   +20%/-10%
    Ceramic   +20%/-10%
     
    >10mm   ±5%
    Ceramic   +20%/-10%
    Polymer   +20%/-10%
     
  Length:   <100mm   ±1mm
    ≥100mm   +5% / -1%